Stack of silicone film-faced MDF panels with a matching wood-grain decor

LAMINATED MDF PANELS

Silicone-Faced Laminated MDF Panels

PVCMelaminePPSilicone

PVC-free film face · One or both sides · Quoted per project

PANEL COMPARISON

Silicone-Faced MDF vs PVC, Melamine, HPL and PET Laminated MDF

Laminated MDF is only as good as its face. Ours is a PVC-free silicone film, flat-laminated to the board, with a soft, leather-like touch and a surface that wipes clean. Here is how it sits next to the faced boards you buy today. If you are still choosing the board itself, start with what laminated MDF is and how MDF is made.

Compare faced-board options, property by property.
What you compare PuremorfilmSilicone-faced MDF PVC-faced MDFMelamine-faced boardHPL-faced boardPET-faced MDF
Touch and feelSoft, skin-like matt touchFinish-dependent; soft-touch grades existHard resin-faced surfaceHard, dense laminateSmooth, hard film face
Everyday cleaning24-hour stains wipe cleanEasy-clean grades availableEasy-clean sealed surfaceStrong everyday stain resistanceWipes clean; gloss shows marks
Scratch resistance2H: no obvious scratchesDepends on protective topcoatHard-wearing; check surface classHard-wearing; check the gradeCoating-dependent; check the grade
Surface wear2,000 cycles; slight mattificationWear-layer dependentGrade-dependent wear classAbrasion-rated grades availableTopcoat-dependent
Heat stability0.06%/0.10% change, 100°C/600-min film testHeat-sensitive film and adhesive systemGrade and exposure-time dependentHeat-resistant grades availableCheck the film and adhesive rating
Flame retardancyFlame-retardant film face as standardDepends on the film formulationDepends on the finished boardFire-rated grades availableCheck the film grade
Ageing over yearsNo DOP; resists embrittlementFormulation-dependent plasticizer migrationStable; grade-dependent appearanceStable resin laminateStable polyester film
Face materialPVC-free, formaldehyde-free filmPVC-based; formulation-dependent additivesMelamine-formaldehyde resin paperResin laminate; low-emission grades existPVC-free polyester film
Faces and edgesFlat-laminated, one or both faces; edges finished separatelyFlat-laminated or 3D-wrapped by gradeBoth faces pressed; edge banding neededBonded face; edge banding neededFlat-laminated; edge banding needed
Compare with:

Silicone vs PVC-faced MDF

Silicone-faced MDF alongside the selected board.
PropertySilicone-faced MDFPVC-faced MDF
Touch and feelSoft, skin-like matt touchFinish-dependent; soft-touch grades exist
Everyday cleaning24-hour stains wipe cleanEasy-clean grades available
Scratch resistance2H: no obvious scratchesDepends on protective topcoat
Surface wear2,000 cycles; slight mattificationWear-layer dependent
Heat stability0.06%/0.10% change, 100°C/600-min film testHeat-sensitive film and adhesive system
Flame retardancyFlame-retardant film face as standardDepends on the film formulation
Ageing over yearsNo DOP; resists embrittlementFormulation-dependent plasticizer migration
Face materialPVC-free, formaldehyde-free filmPVC-based; formulation-dependent additives
Faces and edgesFlat-laminated, one or both faces; edges finished separatelyFlat-laminated or 3D-wrapped by grade

Silicone figures refer to the recorded film specimens. Other columns describe typical board categories; grades and test methods vary. View silicone test conditions. The core board and adhesive are documented separately from the film face.

Put a faced sample next to the board you use now.

Request a Comparison Sample

How a Silicone Face Answers Those Problems

Start with the surface people touch and clean every day, then decide whether you want the film or the finished panel.

Stack of silicone film-faced MDF panels with a matching wood-grain decor

Film and board from one supplier

We print, coat and laminate the film ourselves, so the face on your panel comes from the same production as the film rolls. Panels are faced on the core you specify and quoted per project.

Ask for a Panel Quote →

Judge the face on a real panel before you specify it.

Request Panel Samples

Why Buy Silicone-Faced Panels from Puremorfilm

Most panel suppliers buy their face film from someone else. We make the silicone film ourselves, so the face, the test records and the technical answers come from one place.

Rolls of silicone decorative film on a PET carrier

We make the face, not just the panel

The silicone film is printed, coated and cured on our own six lines, with more than 1 million m² of monthly film capacity. Your panels are faced with film from the same production, and a repeat order uses the same approved reference.

Pencil scratch test on a silicone decorative film sampleWatch video0:22

A PVC-free face with SGS records

The film is PVC-free, formaldehyde-free and No DOP. SGS has tested it for formaldehyde emission, REACH SVHC and RoHS, plus 2H pencil scratch and 2,000-cycle Taber abrasion. You get the reports with your quote.

See the recorded results →
Decorative film lamination trial on an MDF substrate

Engineers who work on the material

Our founding team developed the silicone surface technology behind the film, which is already used in projects for international phone and watch brands and in automotive projection screens. Questions about core, adhesive and edges go to the same R&D team.

Decorative film colour swatches and laminated panel samples

Production MOQ, free samples, custom finishes

Free film and panel sample requests are separate from production orders. Production MOQ: standard film 500 m; panels 200 sheets at 1220 × 2440 mm. Choose from 100+ patterns or develop your own colour, texture and private label, all quoted per project.

See the difference on a real panel before you commit.

Request Free Panel Samples

Panel Manufacturing & Quality Control

See how the face is made, then agree the checks your panel order needs. Watch the factory video

  • 10+years in decorative surface materials
  • 6lines for printing, coating and lamination
  • 1M+ m²monthly film capacity
  • 100+patterns ready to sample

From coated film to faced panel

The silicone face is coated and cured on our own lines, then flat-laminated to the board with PUR adhesive. See the lines running on a live video factory tour.

Silicone film coating line with raw-material tanks in the Puremorfilm factoryFactory video1:15
Coating line
Workers inspecting white base film on a roll inspection table
Roll inspection
Wrapped decorative film rolls staged on the Puremorfilm warehouse floor
Finished film rolls

Quality checkpoints from film to finished panel

Agree the inspection items, tolerances and records against the approved panel sample before production.

  1. 01

    Incoming film & boards

    Film batch, core board grade, flatness and surface condition.

  2. 02

    During lamination

    Colour against the approved sample, bond, bubbles and visible defects.

  3. 03

    Finished panels

    Size, thickness, face appearance and agreed acceptance checks.

  4. 04

    Before dispatch

    Batch labels, quantity, face protection and edge-safe packing.

Shade matching, nonconforming panels & traceability

Each order is checked against the approved reference sample, and panels for one project can be kept to one film batch where the quantity allows. Agree how nonconforming panels are identified, held and rechecked, and which production records travel with the shipment. Request the QC checklist for your order.

Watch the lines on video and tell us what your buyer inspects.

Book a Video Factory Tour Request QC Details

Where Silicone-Faced Panels Are Used

Pick an application to see what buyers check first and what we confirm before sampling.

Matte film-faced kitchen cabinet doors and island fronts

Kitchen and wardrobe doors

Flat doors and carcass panels faced on one or both sides, with the edge treatment planned for the room. See the film itself on our furniture decorative film page.

What matters most
Grease and stains, heat near appliances, sealed edges
What we confirm next
Core board, door size, faces and edge treatment
Ask About Door Panels

Working on a project like one of these? Ask which references we can share.

Discuss a Similar Project

Judge the Look and the Touch with Real Samples

Every finish below can face a panel. Compare wood grain, solid colours and leather textures on screen, then ask for a faced panel sample to see the finish after bonding.

Wood grain

Choose a finish family and hold the faced panel in your hands.

Request Colour Samples

Panel Construction & Supply Options

Tell us the core and size you need, or buy the film and laminate it on your own line.

Stack of silicone film-faced MDF panels with a matching wood-grain decor

Silicone-faced panels, made to your order

Core board
MDF, particleboard, plywood, OSB or other boards that take flat-laminated PVC film
Faces
One or both sides, same or different finishes
Size & thickness
Confirmed per project, in line with standard PVC-faced panel supply
Edges
Edge treatment agreed with the face finish
Quote Laminated Panels
Silicone decorative film roll

Film rolls for your own lamination line

Effective width
1240 / 1260 / 1400 mm, by model
Roll length
50 / 100 / 250 / 500 m, by model
Process
Flat lamination with PUR adhesive
Support
Technical guidance during your lamination trials
See Film Rolls
Why the core is documented separately

The film face is PVC-free, formaldehyde-free and No DOP. Emission, moisture and strength figures for a finished panel also depend on the core board and adhesive, so we name the core grade on the quote and supply its own documents. Ask for a low-emission or moisture-resistant core if your market requires it.

Not sure whether to buy panels or film? Tell us what equipment you run.

Help Me Choose a Supply Form

Film Performance: Recorded Results & Test Conditions

These are results for the silicone film that faces the panel. Review the highlights, then expand the records you need. Whole-panel performance also depends on the core board and adhesive, and is confirmed for your construction.

Pencil scratch

No obvious scratches

2H pencil · 500 gf · 45° · three strokes ≥20 mm. White paper summary of SGS PL02.

Taber abrasion

2,000 cycles

Slight mattification only; no concentrated scratches, exposed backing or coating peeling. CS-10 · 1,000 g per wheel · 60 rpm. SGS PL04 summary.

Thermal dimensional change

0.06% / 0.10%

Length / width after 100°C for 600 minutes and 14-hour room-temperature recovery. SGS PL01 summary.

Source: technical white paper V1.0 (October 2026), including SGS report summaries, laboratory records and patent worked examples. Request the original matching report for the supplied model.

SGS report summaries: four film tests
Test itemRecorded resultTest conditionsSource & scope
Pencil scratchNo obvious scratches2H pencil; 500 gf load; 45° angle; three strokes, each ≥20 mm.SZIN2608002405PL02_EN
26 Aug 2026. Tested film specimen; resistance under these tool and load conditions.
Taber abrasion2,000 cycles: slight mattification only; no concentrated scratches, substrate exposure or coating peeling.ASTM D4060-25; CS-10 wheels; 1,000 g per wheel; 60 rpm.SZIN2608002405PL04_EN
27 Aug 2026. Surface-wear evidence for the tested film; assess against the intended wall or furniture use.
Thermal dimensional stabilityLength change 0.06%; width change 0.10%.100°C for 600 minutes, followed by 14 hours at room temperature. Lab environment: 23±2°C, 50±5% RH.SZIN2608002405PL01_EN
26 Aug 2026. Supports dimensional and processing evaluation of the tested film.
Tensile breaking force & elongationA1: 216.4 N / 51%
A2: 126.3 N / 67%
Specimen thickness: A1 0.473 mm; A2 0.605 mm.
JIS K 6732:1996+AMD.1:2006 and client requirements; 200 mm/min; 40 mm gauge length; 23±2°C, 50±5% RH.SZIN2608002405PL03_EN
27 Aug 2026. N is breaking force. Specimens 1 and 2 broke outside the gauge marks; those results are for reference only.
Laboratory records: stains & cleaning
Test itemRecorded resultTest conditionsSource & scope
Food, drink & cosmeticsNo visible change after wiping: coffee, red wine, ice cream, soy sauce, Worcestershire sauce and lipstick.Contaminants applied to the film surface; held at 25°C for 24 hours, then wiped.Laboratory data, white paper §6.2. Results apply to the stated exposure and wiping method; match cleaners to the supplied grade.
Pen & marker marksNo visible change or slight staining: ballpoint pen, water-based marker and oil-based marker.Same recorded method: 25°C for 24 hours, followed by wiping.Laboratory data, white paper §6.2. The recorded result varies; confirm the contaminant-specific result for the chosen film.
Patent worked examples: interlayer stability & antibacterial grade
Test itemRecorded resultTest conditionsSource & scope
Internal film interlayer peelBOPET system: ≥3 N/15 mm
TPU system: ≥3.5 N/15 mm.
180° peel; BOPET backing 125 μm and TPU backing 200 μm.Patent worked examples 1 and 2, white paper §5.4. Internal film interface only; does not establish film-to-board adhesive strength.
Damp-heat ageingNo delamination or blistering.85°C / 85% RH for 500 hours.Patent worked-example data, white paper §5.4. Confirm the corresponding construction for supply.
Thermal cyclingNo delamination or blistering.−40°C to 85°C; 100 cycles.Patent worked-example data, white paper §5.4. Applies to the evaluated example construction.
Boiling-water exposureNo delamination or blistering.Boiling water for 12 hours.Patent worked-example data, white paper §5.4. Confirm film grade and construction.
Antibacterial reduction≥99% against Escherichia coli and Staphylococcus aureus.Recorded for an antibacterial worked-example formulation. Confirm formulation grade and corresponding test conditions.Patent worked-example data, white paper §9. Antibacterial performance is grade-specific; request evidence for the supplied model.
Surface wettabilityWater contact angle approximately 108° in the worked example; stated range 100°–115°.Worked-example surface measurement; full measurement conditions to be matched to the grade.Patent worked-example data, white paper §6.1. A wettability measure for the evaluated surface.
Additional laboratory records: weathering & exposure
Test itemRecorded resultTest conditionsSource & scope
Accelerated ageingNo visible change after 2,000 hours.White paper records JIS B7753 light and water exposure testing.Laboratory data, white paper §7.2. Confirm the original exposure program and film grade for a weathering specification.
Yellowing resistanceGrade ≥4.QUV-A testing, as recorded; duration and grading details to be confirmed with the matching test record.Laboratory data, white paper §7.2. Compare only with a matching procedure and grading scale.
Hydrolysis exposureRecorded duration ≥10 weeks.85°C / 85% RH.Laboratory data, white paper §7.2. Request the appearance/strength acceptance criteria for the specified grade.
Salt-spray exposureRecorded duration ≥1,000 hours.ASTM B117, as recorded in the white paper.Laboratory data, white paper §7.2. Project acceptance criteria and the post-exposure result are confirmed separately.
Water stainingClass 5.ISO 105-E01 / ASTM D1735-2021, as recorded.Laboratory data, white paper §7.2. Confirm the grading procedure and specimen.
Perspiration stainingClass 5.ISO 11641:2012 / ISO 105-E04, as recorded.Laboratory data, white paper §7.2. Confirm the intended contact conditions and film grade.
Material safety & fire performance for panels

The film face is PVC-free, formaldehyde-free and No DOP, and has been tested by SGS for formaldehyde emission, REACH SVHC and RoHS. On a laminated panel, the core board and adhesive carry their own emission documents, which we supply with the quote.

The silicone surface is inherently flame-retardant, and higher grades up to UL 94 V-0 can be made on request. A panel fire classification depends on the film, adhesive and core together, so name the standard you need and we will confirm the construction.

Develop a Panel Finish for Your Collection

Send a reference colour, grain or design file. We check feasibility and terms before proofing it on film and on your chosen core.

Colour & pattern

Match a colour code, a wood grain or your own artwork across a furniture range.

Texture & gloss

Choose the grain, gloss level and hand feel, then compare them on a physical panel proof.

Panel & labelling

Agree core, size, faces, packing and any private-label marking for your distributors.

Design brief → Feasibility & terms → Panel proof → Approved production reference

Have a finish reference? Add it to your inquiry.

Discuss a Custom Finish

Plan the Face, Adhesive, Core & Edges Together

A faced panel is a system. Tell us where it will be used, and we match the film grade, adhesive and core to it before you order in volume.

What goes into one silicone-faced panel

  • Silicone surface and functional layersTouch, cleaning and wear
  • Bonding layer and base filmColour and pattern on a PET base film
  • PUR adhesive layerFlat-laminated to the board
  • Substrate panelMDF, particleboard, OSB, honeycomb or other cores
Panel performance depends on every layer and on the lamination, so we evaluate them together.

What to tell us

  • Core boardBoard type, grade and thickness
  • Room conditionsMoisture, heat sources and cleaning agents
  • Faces and edgesOne or two faces, and how the edges are finished
  • Panel listSizes, quantities and any cutting allowance
  • Acceptance criteriaThe appearance, bond and documents your buyer will check
Three checks before you switch your panel face
  • Approve the face on a panel sample, not only a film swatch.
  • Check the edges and cut-outs on a trial component; internal film peel data is a different measurement.
  • Agree the documents for the core and adhesive as well as the film.

Send your panel list and conditions. We will check the construction before you order in volume.

Submit My Panel Requirements

What Goes Into a Panel Quotation

Panels are quoted per project. The more of these you can share, the faster the quote comes back.

Board

Core type, grade, thickness and panel size.

Face

Finish, one or two faces, and edge treatment.

Packing

Face protection, edge guards and pallet build.

Delivery

Quantity, destination, freight and schedule.

For a useful quote: send the application, core board, panel size and thickness, faces, estimated quantity and destination. Add your preferred finish if you have one.
MOQ, samples and lead time

For production orders, panels are 1220 × 2440 mm with a minimum of 200 sheets; standard film starts at 500 m. Sample requests are separate, and samples are free. Panel prices depend on the core, size, faces, finish and quantity. Lead time follows standard practice for PVC-faced panels and is confirmed on the quote, together with packing and freight.

Share what you know now. Anything missing can be settled during sampling.

Get a Panel Quote

From Panel Sample to Checked Shipment

Approve the face and construction first, then lock in production and delivery.

  1. 01

    Choose & sample

    Pick a finish and receive free film and panel samples.

  2. 02

    Confirm the construction

    Agree the core, faces, edges, sizes, acceptance criteria and quantity.

  3. 03

    Laminate & inspect

    Panels are faced, checked against the approved sample and recorded by batch.

  4. 04

    Pack & dispatch

    Faces protected, edges guarded, documents and freight arranged.

Trial panels before a volume order

For a new project, use panel samples to check cutting, edging and assembly on your own line before a production order. Sample requests are separate from production orders; production panels are 1220 × 2440 mm with a minimum of 200 sheets. Timing is confirmed with the quote.

Start with a sample set and the checks you want to run.

Start Panel Evaluation

Before You Sample & Order Panels

Common questions from furniture makers, distributors and project buyers.

Are these laminated MDF panels PVC-free?

The face is. It is a crosslinked silicone surface on a PET base film, with a No DOP formulation and no PVC. The core underneath is MDF or another board you choose.

Are the panels formaldehyde-free?

The film face is formaldehyde-free and has been tested by SGS for formaldehyde emission. Panel emissions also depend on the core board and adhesive, so we name the core grade on the quote and supply its own documents. Ask for a low-emission core if your market requires one.

Which core boards can you face?

MDF, particleboard, plywood, OSB, honeycomb and other boards that can take flat-laminated PVC film. Panels can be faced on one side or both.

What sizes, thicknesses and lead times do you offer?

They follow standard practice for PVC-faced panels and are confirmed for each project on the quote. Send your panel list and we will reply with the construction, lead time and packing.

Is there a minimum order quantity?

Yes. For production orders, panels are 1220 × 2440 mm with a minimum of 200 sheets; standard film starts at 500 m. Sample requests are separate and samples are free. Panels are quoted per project.

Can I buy the film and laminate it myself?

Yes. Film rolls are our main supply. They are flat-laminated with PUR adhesive, and we give technical guidance during your trials. See our furniture decorative film page.

Where should silicone-faced panels not be used?

The surface has a leather-like feel and some give, so it is not suited to floors, worktops, stovetop areas, shower floors or other surfaces people walk on.

Have a question not covered here? Our technical team will answer it directly.

Ask a Technical Question

Request Laminated MDF Panel Samples or a Quote

Ask for free panel samples, a project quote or test documents. Share the core, size and finish if you know them; only your email is required.

Decorative film colour swatches and laminated panel samples for selection
  • Free panel samples and colour swatches
  • Film test summaries and core-board documents
  • A quote for your core, size and faces

Request samples or advice

Choose what you need. Only your email is required.

Enter a valid email so we can reply.

What would you like?
Add company, quantity, specification or files

    We reply by email with the samples, documents or quote you asked for.

    We only use your email to reply to this request.

    Puremorfilm video