PVC-free composition
No PVC, no added formaldehyde and a No DOP formulation in the film. Confirm the adhesive and core board separately.

A new, eco-friendly
surface material.
Puremorfilm is a Chinese manufacturer of silicone decorative film and silicone laminated panels, with a silicone functional surface on a PET support film. We supply rolls without a self-adhesive backing for PUR flat lamination, or laminated panels quoted per project, for furniture fronts, cabinet doors, wall panels and other vertical or low-wear surfaces; neither supply form is suitable for floors, countertops or stovetops.
PVC-freeNo added formaldehydeNo DOP
A NEW SURFACE, TWO SUPPLY FORMS
A crosslinked silicone surface on a PET support film. It brings a soft touch and an easy-clean decorative finish to furniture and interiors.
Choose film rolls for your own lamination, or laminated panels with the surface already bonded to a core board. PVC-free, with no added formaldehyde and a No DOP formulation in the film; panel construction is confirmed separately.
A soft-touch finish with a PVC-free composition, practical surface protection and a choice of decorative effects.
No PVC, no added formaldehyde and a No DOP formulation in the film. Confirm the adhesive and core board separately.
Watch videoVIDEO0:32
Our silicone decorative film is flame retardant. Request the relevant test report for your application and panel construction.
Watch cigarette-contact video
Watch videoVIDEO0:22
A finish for furniture fronts, desk modesty panels and wall panels. Check the measured result against your contact and load conditions.
Watch scratch video
Watch videoVIDEO0:23
A soft decorative surface that helps simplify daily care. Confirm the stain, exposure time and cleaner for your selected grade.
Watch cleaning videoFilm results apply to the tested grade and conditions. For a laminated panel, the film, adhesive and core board form one construction and need their own assessment. The silicone film is flame retardant. Fire classifications apply to the tested construction; stain and scratch results depend on the stated method.
The technical white paper records a 2H pencil test at 500 gf and a Taber test at 2,000 cycles. Matching methods, specimen details and records are provided in the quality-control section below.
Compare surface feel, cleaning, composition, flame retardancy and long-term stability before choosing your next finish.
| Buyer question | Silicone decorative film | PVC decorative film | Melamine-impregnated paper | Printed PP decorative film | Painted surface |
|---|---|---|---|---|---|
| Soft to the touch? | Yes: Soft, skin-like touch | Partly: Smooth plastic surface | No: Hard surface feel | Partly: Plastic surface feel | Partly: Feel depends on the coating |
| Easy to wipe clean? | Yes: Clean with water and a damp cloth | Partly: Dirt can collect in textured grooves | Yes: Smooth surfaces wipe clean easily | Partly: Cleanability depends on the protective coating | Varies: Matte coatings can show stains |
| No added formaldehyde? | Yes: No formaldehyde added | Yes: Usually no formaldehyde added | No: Uses melamine-formaldehyde resin | Yes: Usually no formaldehyde added | Partly: Depends on the coating formulation |
| No DOP? | Yes: No DOP | Check: DOP content depends on the formulation | Yes: No DOP (typically) | Yes: No DOP (typically) | Partly: Depends on the coating formulation |
| Is the silicone surface flame retardant? | Yes: Inherently flame retardant | Partly: Depends on the film formulation | Partly: Depends on the finished board | No: Requires flame-retardant treatment | Partly: Depends on the coating and substrate |
| Resists yellowing and brittleness? | Yes: Stable for years; no yellowing or brittleness | No: Can turn yellow and become brittle | Varies: Ageing depends on the resin and finish | Partly: Ageing depends on the film and coating | Partly: Some light-coloured coatings can yellow |
Silicone decorative film is available in woodgrain, leather, stone, solid-colour and custom designs.
The silicone column describes our decorative film. Other materials vary by formulation and finish. Laminated-panel performance also depends on the adhesive and core board.
Find the surface you need for the part you make. Film grade, substrate and processing are selected for the actual application.
Desk fronts, storage and office furniture panels with a soft, wipe-clean surface.
Soft-touch decorative surfaces for wardrobe, kitchen and bathroom cabinet doors.
Furniture fronts, storage and wall surfaces for children's rooms and early-learning spaces.
Decorative wall panels for homes, with wood, stone and solid looks.
Furniture, wall panels and display cabinets for hotels, retail and commercial interiors.
Desk fronts, partitions and storage that resist scratches and everyday marks.
Tell us the contact, cleaning and exposure conditions. We review the film grade, substrate and processing method against your requirements. Floors and kitchen worktops are outside our standard recommended uses.
Tell us the part, contact conditions and environment. We will help select a suitable film or panel.
Choose the supply form that fits your equipment and purchasing plan.
Flexible film for your own lamination or bonding. Add the silicone finish to your existing substrate and production flow.
Supplied as panels
Boards with the silicone surface already bonded to a selected core. Confirm the construction before cutting and machining.
Whole-panel performance is confirmed for the actual combination of film, adhesive and core board.
From application evaluation to repeat supply, our team helps turn a new surface material into a workable product specification.

Discuss the surface, substrate and process with our R&D team before choosing a grade.
Automotive and mobile-phone applications include volume production, alongside development work in wearables and projection.
Printing, coating and lamination capacity supports repeat orders to an agreed specification.
Approve samples, specifications and acceptance criteria before bulk production. Confirm the schedule for your order.
Typical lead times are confirmed for each order. Custom patterns require an additional 7–10 days for proofing and approval.
CUSTOMER FEEDBACK
Feedback on touch, processing, cleaning and technical support. Customer names are withheld at their request.
We switched our children's furniture line to Puremorfilm film. The soft-touch surface was the first thing our retail buyers noticed, and the formaldehyde-free test reports made our compliance review much faster.
The film ran on our existing lamination line after one trial. Color consistency between batches has been reliable, and the pre-shipment photos save us a lot of back-and-forth.
Teachers told us crayon marks on the wall panels wipe straight off. For spaces where children touch everything, that is exactly what we needed.
The custom wood grain we developed with their team now sells as our own private-label range. Samples arrived quickly and the swatch book helps our dealers close orders.
We needed a leather-like strap material that feels soft on the skin and stays clean. Their team adjusted the texture and thickness until it matched our design.
We evaluated the silicone surface for door trims. Touch, scratch behavior and cleanability met our internal targets, and the documentation was well prepared.
A clear sequence of decisions, from material selection to delivery.

Share your application, supply form, substrate and surface requirements.
Confirm the film or panel direction, sample options and quotation basis.
Check colour, texture and touch; run a lamination trial where needed.
Agree the pattern, specification, quantity and acceptance criteria.
We make the order to the approved specification and check the batch.
Confirm labels, protection, documents, destination and shipping terms.
Sample dispatch: 3–5 working days. Standard bulk production: 15–25 days after deposit. Custom patterns add 7–10 days for proofing and approval. Final timing is confirmed for each order.
Approve the reference sample, check the production batch and review the documents for the grade you are buying.

No obvious scratches
2H pencil · 500 gf · 45° · three strokes ≥20 mm. White paper summary of SGS PL02.
2,000 cycles
Slight mattification; no concentrated scratches, exposed backing or peeling. CS-10, 1,000 g per wheel, 60 rpm. SGS PL04 summary.
0.06% / 0.10%
Length / width after 100°C for 600 minutes and 14-hour room-temperature recovery. SGS PL01 summary.
Source: technical white paper V1.0 (October 2026). SGS report summaries, laboratory records and patent worked examples are identified below. Results apply to the tested specimens and conditions; request the record matching your grade.
| Test item | Recorded result | Test conditions | Source & scope |
|---|---|---|---|
| Pencil scratch | No obvious scratches | 2H pencil; 500 gf load; 45° angle; three strokes, each ≥20 mm. | SZIN2608002405PL02_EN 26 Aug 2026. Tested film specimen; resistance under these tool and load conditions. |
| Taber abrasion | 2,000 cycles: slight mattification only; no concentrated scratches, substrate exposure or coating peeling. | ASTM D4060-25; CS-10 wheels; 1,000 g per wheel; 60 rpm. | SZIN2608002405PL04_EN 27 Aug 2026. Surface-wear evidence for the tested film; assess against the intended wall or furniture use. |
| Thermal dimensional stability | Length change 0.06%; width change 0.10%. | 100°C for 600 minutes, followed by 14 hours at room temperature. Lab environment: 23±2°C, 50±5% RH. | SZIN2608002405PL01_EN 26 Aug 2026. Supports dimensional and processing evaluation of the tested film. |
| Tensile breaking force & elongation | A1: 216.4 N / 51% A2: 126.3 N / 67% Specimen thickness: A1 0.473 mm; A2 0.605 mm. |
JIS K 6732:1996+AMD.1:2006 and client requirements; 200 mm/min; 40 mm gauge length; 23±2°C, 50±5% RH. | SZIN2608002405PL03_EN 27 Aug 2026. N is breaking force. Specimens 1 and 2 broke outside the gauge marks; those results are for reference only. |
| Test item | Recorded result | Test conditions | Source & scope |
|---|---|---|---|
| Food, drink & cosmetics | No visible change after wiping: coffee, red wine, ice cream, soy sauce, Worcestershire sauce and lipstick. | Contaminants applied to the film surface; held at 25°C for 24 hours, then wiped. | Laboratory data, white paper §6.2. Results apply to the stated exposure and wiping method; match cleaners to the supplied grade. |
| Pen & marker marks | No visible change or slight staining: ballpoint pen, water-based marker and oil-based marker. | Same recorded method: 25°C for 24 hours, followed by wiping. | Laboratory data, white paper §6.2. The recorded result varies; confirm the contaminant-specific result for the chosen film. |
| Test item | Recorded result | Test conditions | Source & scope |
|---|---|---|---|
| Internal film interlayer peel | BOPET system: ≥3 N/15 mm TPU system: ≥3.5 N/15 mm. |
180° peel; BOPET backing 125 μm and TPU backing 200 μm. | Patent worked examples 1 and 2, white paper §5.4. Internal film interface only; does not establish film-to-board adhesive strength. |
| Damp-heat ageing | No delamination or blistering. | 85°C / 85% RH for 500 hours. | Patent worked-example data, white paper §5.4. Confirm the corresponding construction for supply. |
| Thermal cycling | No delamination or blistering. | −40°C to 85°C; 100 cycles. | Patent worked-example data, white paper §5.4. Applies to the evaluated example construction. |
| Boiling-water exposure | No delamination or blistering. | Boiling water for 12 hours. | Patent worked-example data, white paper §5.4. Confirm film grade and construction. |
| Antibacterial reduction | ≥99% against Escherichia coli and Staphylococcus aureus. | Recorded for an antibacterial worked-example formulation. Confirm formulation grade and corresponding test conditions. | Patent worked-example data, white paper §9. Antibacterial performance is grade-specific; request evidence for the supplied model. |
| Surface wettability | Water contact angle approximately 108° in the worked example; stated range 100°–115°. | Worked-example surface measurement; full measurement conditions to be matched to the grade. | Patent worked-example data, white paper §6.1. A wettability measure for the evaluated surface. |
| Test item | Recorded result | Test conditions | Source & scope |
|---|---|---|---|
| Accelerated ageing | No visible change after 2,000 hours. | White paper records JIS B7753 light and water exposure testing. | Laboratory data, white paper §7.2. Confirm the original exposure program and film grade for a weathering specification. |
| Yellowing resistance | Grade ≥4. | QUV-A testing, as recorded; duration and grading details to be confirmed with the matching test record. | Laboratory data, white paper §7.2. Compare only with a matching procedure and grading scale. |
| Hydrolysis exposure | Recorded duration ≥10 weeks. | 85°C / 85% RH. | Laboratory data, white paper §7.2. Request the appearance/strength acceptance criteria for the specified grade. |
| Salt-spray exposure | Recorded duration ≥1,000 hours. | ASTM B117, as recorded in the white paper. | Laboratory data, white paper §7.2. Project acceptance criteria and the post-exposure result are confirmed separately. |
| Water staining | Class 5. | ISO 105-E01 / ASTM D1735-2021, as recorded. | Laboratory data, white paper §7.2. Confirm the grading procedure and specimen. |
| Perspiration staining | Class 5. | ISO 11641:2012 / ISO 105-E04, as recorded. | Laboratory data, white paper §7.2. Confirm the intended contact conditions and film grade. |
Puremorfilm makes silicone decorative film and laminated panels in China. Base-film extrusion, coating, embossing, slitting and flat lamination run on our own lines.
Watch videoFACTORY FILM1:15
ON THE PRODUCTION FLOOR
Take a closer look at the people, equipment and processes behind our silicone leather and functional films.
Watch the factory filmSee our production lines on a live video factory tour or an on-site visit.
Polymer pellets for the base film.
The base film is extruded from the pellets.
An online gauge measures thickness across the film.
The extruded film is wound into rolls.
The silicone surface is coated onto the base film.
Rolls are slit to the ordered width.
Rolls are wrapped, palletised and shipped.
Our team's materials development and validation work covers consumer electronics, automotive interiors, wearables and projection. Automotive and mobile-phone applications include volume production.
3C cover-material development and validation for a major Chinese technology manufacturer.
Automotive materials work for premium new-energy SUV and executive-sedan programs.
Projection-screen materials work for a smart-projection equipment brand.
Phone-cover materials development and validation for an international mobile-phone brand.
Materials work on a cloud-effect, light-transmitting automotive decorative series.
Soft-touch, wipe-clean strap and wearable surface materials developed for watch brands.
For a new project, the supply specification and validation scope are agreed for the intended application. Marine and outdoor uses require review of the relevant project requirements.
Explore wood, leather, fabric, stone and solid finishes, or develop a pattern for your product line.






Develop a finish for your product line. Send a reference, review the proof sample and approve the specification before bulk production.

Have a pattern, color or spec in mind? Start a custom project.
Confirm the supply specification and the complete processing system before ordering.
| Item | Film rolls | Laminated panels |
|---|---|---|
| Effective film width | 1240 / 1260 / 1400 mm | Panel size: 1220 × 2440 mm |
| Roll length | 50 / 100 / 250 / 500 m | Supplied as finished panels |
| Support film | PET support film as standard production; the visible surface is always silicone. PC, TPU and other support films for development projects. | Film grade matched to the core board and application |
| Thickness | Total composite-film thickness and tolerance confirmed by grade | Core material and board thickness confirmed for the order |
| Back adhesive | Standard film is supplied without back adhesive. Discuss adhesive requirements with us. | Film bonded to a selected core board; construction confirmed separately |
| Surface options | Wood, leather, fabric, stone, solid colours and other textures; gloss and functional grade selected by application | |
Dimensions and material options are recorded in the technical white paper, V1.0. Available width, roll length, backing and surface combinations are confirmed for the selected model.

Identify the core board or substrate and the intended adhesive. Standard film has no back adhesive; trial the complete bonding system.
Share the lamination method, temperature and part geometry. Evaluate representative edges, corners and openings before production.
Agree colour, texture, dimensions and performance criteria. Film interlayer data does not establish film-to-board bond strength.
Agree how the goods will be protected, shipped and quoted for your order and destination.


Rigid cores, protective foam or wrapping, and reinforced ends protect film rolls. Cartons or secured pallets suit bulk shipments; panels use edge protection and separators.
Commercial invoice and packing list match the shipment. Confirm any certificate of origin, transport document or applicable test report needed for your destination.
Sea freight suits bulk orders; air freight or express courier can suit samples and urgent smaller orders. EXW, FOB or CIF terms are confirmed in the quotation.
Confirm product labels, roll or panel condition, carton counts and pallet protection. Request packing photos before loading and keep shipment records for receiving checks.
Film grade and supply form · Pattern or custom development · Width, length, board construction and quantity · Packing protection · Destination, freight and EXW, FOB or CIF terms.
Share these details so material, processing, packing and transport can be quoted on the same basis.
Send the supply form, quantity and destination for your project quotation.
Answers about samples, order quantities, timing, custom work and material selection.
Have a question that is specific to your project?
Ask About My RequirementsA new surface material: a crosslinked silicone surface on a PET support film. It replaces PVC films, melamine paper and printed PP films on furniture, wall panels and other surfaces — with no formaldehyde, a No DOP formulation and a soft, wipe-clean finish.
Yes. The film is PVC-free and uses a No DOP formulation. Request ageing data for the selected grade.
We are a manufacturer. Pattern printing, silicone coating, curing and lamination run on our own production lines in China. Video factory tours and on-site visits are welcome.
Film rolls are for your own lamination or wrapping line. Laminated panels arrive with the film already bonded to a core board, ready to cut and use.
Yes. Send artwork, a physical sample or a color code, and we develop and proof the pattern for your approval. Thickness, width, base film and texture can also be customized.
Standard film rolls start at 500 m; laminated panels are 1220 × 2440 mm and start at 200 sheets. Custom finishes are available on request. Several patterns can be combined in one order.
Samples ship within 3–5 working days. Bulk orders of standard patterns take 15–25 days after deposit; custom patterns add 7–10 days for proofing and approval.
Yes. We send a swatch book and A4 samples of the patterns you choose. A4 samples and the swatch book are free; you only cover express shipping.
Film properties and whole-panel properties are stated separately. For laminated panels, the adhesive and core board are confirmed with matching test reports.
Our quality system is certified to ISO 9001 and ISO 14001, and our film grades are tested by SGS for formaldehyde emission, REACH SVHC and RoHS. Flame-retardancy reports are available for selected grades. Copies are sent on request for the grade you are evaluating.
Wipe with a damp cloth or mild household cleaner. For special stains or strong cleaners, check the care guide or ask us first.
Explore practical guides to decorative film selection, surface performance, lamination and quality control. Make informed material decisions for furniture and interior projects.
Explore more decorative film insights and application guides.
Visit Our Knowledge CenterRequest samples, a quotation, technical documents or an application review. Tell us what you already know; only your email is required.

We will contact you based on the information you provided. In the meantime, you can keep exploring film rolls, laminated panels and applications.
Continue browsing products